Causes and solutions of early pitting corrosion of reducer gear!

Author: China weigao Gearbox     Publish Time: 05-09-2021      Origin: China weigao Gearbox

Inquire

facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button
Causes and solutions of early pitting corrosion of reducer gear!

During the long-term operation of the reducer gear equipment, some special conditions may lead to the early pitting of the equipment. What is the reason for the early pitting of the reducer gear during the use of the equipment, and how should we solve this situation?
1、 Causes of early pitting corrosion of reducer gear equipment
1. The correct selection of selected gear materials and the matching of service load are the reasons for the early pitting corrosion. Secondly, the selection and matching of heat treatment hardness will also lead to the early pitting corrosion of its equipment.
2. Lubricating oil also has a great impact on the early pitting corrosion of reducer gear. The unreasonable lubrication of gear transmission and improper selection of lubricant are also the reasons for the early pitting corrosion of its equipment.
2、 Methods of preventing early pitting corrosion of reducer gear equipment
1. Reasonably lubricate the gear equipment of the reducer and select the lubricant suitable for the equipment.
2. Improve the installation accuracy of the reducer gear, and ensure the contact accuracy of the gear during the operation of the equipment.
For the gear of the reducer, problems during installation and assembly or failure to work according to the normal operation process will easily lead to various fault problems in the operation of the equipment. Therefore, in order to avoid possible problems in the use of the equipment, we must use the equipment according to the normal operation process, At the same time, it is also necessary to maintain the equipment during normal use to avoid its failure.

Latest News

WeiGao Transmission

Weigao Gear Reducer is an alliance group company that integrates research and development, production, sales, and service

+86 400 801 9158

Email: sales@wgt.net.cn;wgt.net.cn@gmail.com
Tel:+86571 85023000

WEIGAO REDUCER

FEEDBACK