How to solve the early pitting corrosion of reducer. Pitting corrosion must be related to lubricating oil, and it should also be closely related to the material of reducer. The normal use process will have certain processing specifications. Another point is caused by the local overload caused by poor gear contact. The local overload of the gear makes the actual contact stress greatly exceed the allowable contact stress of the gear material. Some gears can not reach the full tooth length contact, or only contact at one end of the tooth, or even diagonal contact. The following is a detailed description of Shanghai Jinchuan reducer for us.
1、 Impact of material and handling specifications
The correct selection of gear material, the matching of service load and the selection and matching of heat treatment hardness are also the reasons affecting the early pitting corrosion.
2、 Influence of lubricating oil
The unreasonable lubrication of gear transmission and the improper selection of lubricant are also the reasons affecting the early pitting corrosion. Ways to prevent early pitting corrosion of reducer gear:
(1) Reasonable lubrication of gear reducer transmission and selection of appropriate lubricant.
(2) Improve the gear installation accuracy of the reducer and ensure the contact accuracy of the gear.
For the center drive reducer, if it is not well investigated during assembly and installation, there may be asynchrony between the left and right transmission and poor load sharing effect. In this case, the transmission gear on one side may not bear the load, while the transmission gear on the other side is overloaded (up to twice the design load), which is easy to cause progressive early pitting corrosion on the tooth surface. For more information, welcome to Shanghai Jinchuan reducer for consultation.
Offshore Wind Vessel Gearbox Market 2027: Crane and Winch Drive Demand
Lubrication and maintenance characteristics of B series industrial gearboxes
What are the common misunderstandings in B series gearbox maintenance?
Apron Feeder Gearbox Selection: Chain Pull, Shock Load and Service Factor
How does the R series helical gear reducer perform in a strong vibration environment Selection
Pneumatic Conveying Gearbox Market 2027: Blower, Airlock and Screw Drive Demand
Pellet Mill Gearbox Selection: Ring Die Torque, Thermal Rating and VFD Restart
Is there any way to reduce the parallelism error of the reducer?
Food and Beverage Gearbox Market 2027: Renovation Demand and Mixer Sizing
Marine Deck Winch Gearbox Selection: Drum Torque, Duty Class and Holding Brake
What specific damage will reversal with load cause to the BWY27-59-4KW cycloidal pinwheel reducer?
How to avoid XLED32-841-0.37KW cycloidal pinwheel reducer with load reversal
Desalination Plant Gearbox Market 2027: SWRO Pump Drive Demand
What are the common problems with NGW42-25 planetary reducer base welding?
What kind of noise will the reducer produce if the box manufacturing accuracy is not up to standard?
Slewing Drive Solar Tracker Selection: Wind Load and Holding Torque
Which is more efficient, cycloidal pinwheel reducer or worm gear reducer?