WeiGao Transmission
Email: sales@wgt.net.cn
Language
通栏图2
tonglantu.jpg
Home / News / How to distinguish between gear tooth surface gluing and pitting corrosion: key points of identification and preventive measures - Hangzhou Weigao Transmission

How to distinguish between gear tooth surface gluing and pitting corrosion: key points of identification and preventive measures - Hangzhou Weigao Transmission

Author: Site Editor     Publish Time: 25-10-2026      Origin: Site

Inquire

facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

Why should we distinguish between gear tooth surface gluing and pitting corrosion?

Among reducer gear failures, pitting corrosion and gluing are the two most easily confused types of damage, but they have completely different causes. Reducer gear pitting is contact fatigue, and its development is measured in months or years; tooth surface gluing is the metal adhesion and tearing off after the oil film breaks, and it may only take a few hours from occurrence to scrapping. Distinguish between the two clearly and directly determine the maintenance decision: most pitting corrosion can be monitored and continued to be used, while gluing often requires immediate shutdown.

Essential difference: fatigue accumulation and instant failure of oil film

The mechanism of pitting corrosion is the initiation of fatigue cracks on the tooth surface under alternating contact stress. The pitting gradually expands from the size of the needle tip, which is a progressive damage. When the rotation speed and load remain unchanged, the service life can be estimated according to the fatigue curve. The mechanism of gluing is that the instantaneous temperature in the meshing area is too high or the oil film strength is insufficient. Solid-phase welding occurs on the two tooth surfaces. When the gear continues to rotate, the sticking point is torn apart, forming a tear groove along the sliding direction. This is not fatigue, but lubrication failure. Therefore , it has nothing to do with the running time and is strongly related to the working conditions, oil quality and oil temperature.。

Three judgments: location, appearance and development speed

discriminant dimension

Pitting corrosion

glued

Damage location

Mainly near the node line (sliding speed is small)

Tooth top and root (high sliding speed), pitch lines are usually intact

Appearance

Smooth shell-like pits with clear edges

Grooves and tears along the sliding direction, visible material transfer

Development speed

Months to years, can be monitored

It can last from a few minutes to a few hours.

oil signal

Large particles slowly increase

Sudden increase in iron content and large particles

Tips for quick on-site judgment: if the pit is on the pitch line and the pit wall is smooth, it is pitting corrosion; if the damage is on the top and root of the tooth, there are scratches and chips, it is glue. If in doubt, take a photo of the tooth surface and keep an oil sample for subsequent judgment during reducer maintenance .

Three common causes of gluing

The first is thermal bonding: under high-speed and heavy-load conditions, the flash temperature exceeds the critical temperature of the oil film, which is common in the meshing area between the pinion tooth root and the large gear tooth top of the hard-tooth surface reducer. The second is cold gluing: the oil film is too thin when the speed is high and the oil viscosity is low, especially during the running-in period of new equipment. The third is lubrication management errors: wrong oil ( worm gear reducer misuses ordinary gear oil), insufficient oil volume, oil temperature exceeding 80°C for a long time, and failure to change the oil on schedule after the extreme pressure additive is exhausted.

Preventive measures: Three-pronged approach of oil, heat dissipation and running-in

measure

Specific practices

Choose the right oil

For heavy loads, choose gear oil containing sulfur and phosphorus extreme pressure agents to allow the reducer lubricant to form a sufficient oil film thickness; for the worm gear pair, choose an oil-based worm gear oil; check the viscosity grade according to the instructions

Control oil temperature

The temperature of the oil pool should be stable within 80°C. If it exceeds the limit, check the oil level, heat sink and ventilation cap, and install a fan if necessary.

Standard running-in

After the machine is new or overhauled, run it at half load for about 10 hours to allow the tooth surface to run in to produce a smooth contact zone, and then run it at full load.

Surfaces and Geometry

Gear grinding reduces roughness, tooth profile modification improves bite impact, and nitriding treatment is optional during reshaping to improve anti-gluing ability.

Slight gluing (shallow scratches, no peeling) can be used to grind burrs, clean and change oil, and then reduce load and observe; when pieces of material transfer or deep tears occur, the tooth surface cannot be repaired. The gear pair should be replaced and the oil and heat dissipation root causes should be investigated to avoid the same damage in new parts.

Hangzhou Weigao Transmission produces a series of such as hard tooth surfaces, cycloid pinwheels, worm gears, etc. reducers and gear reduction motors It supports free calculation of oil viscosity and thermal power according to working conditions, helping customers avoid pitting corrosion and gluing risks from the source. If you are looking for a reliable reducer manufacturer , or need reducer Selection consultation and failure analysis support, please contact our technical team to obtain Selection solutions.

Latest News

Random Products

WeiGao Transmission

Weigao Gear Reducer is an alliance group company that integrates research and development, production, sales, and service

+86 400 801 9158

Email: sales@wgt.net.cn;wgt.net.cn@gmail.com
Tel:+86571 85023000

WEIGAO REDUCER