Can the moderate burn on the tooth surface of the 30KW TY112-40 reducer be repaired?

Publish Time: 2026-10-10     Origin: Site

1. Mainstream repair solutions adapted to this model

‌1. Laser cladding local strengthening repair‌

This is the preferred solution under 30KW heavy-load conditions: Alloy powder that matches the gear base material is fed into the laser beam simultaneously to form a high-hardness cladding layer of 0.2~0.5mm on the burnt and peeled tooth surface. The heat-affected zone is only 0.1~0.3mm, which will not damage the internal metallographic structure of the gear. The bonding strength can reach more than 90% of the base material. After repair, the tooth surface hardness can be restored to HRC55~60, which is suitable for the heavy-duty transmission requirements of this model.

2. ‌Partial surfacing + precision grinding repair‌

For moderate burns caused by partial spalling, Cr-Mo wear-resistant electrodes were selected. The gears were preheated to 200°C before welding, and the tooth surface defects were repaired by layered surfacing. Stress relief annealing was performed immediately after welding, and then the tooth shape was ground by a form grinder according to the original module and pressure angle parameters to ensure that the tooth pitch deviation was controlled within the level 7 accuracy of GB/T 10095.

‌3. Brush plating + tooth surface modification and repair‌

If the burn only causes the hardness of the shallow layer of the tooth surface to decrease and the wear amount is in the range of 0.1~0.5mm, the surface softening layer can be removed by grinding first, and the tooth surface size can be restored by depositing a nickel-based alloy coating through brush plating. The hardness of the coating can reach above HRC45, and then manually modified with a whetstone, and the meshing contact spots can be checked with red red powder to ensure that the contact area is not less than 60% of the tooth surface.

2. Assessment must be done before repair and the boundary of irreparable

First, use magnetic particle/ultrasonic non-destructive testing to check whether deep cracks extend on the tooth surface. Use a hardness tester to confirm whether the hardened layer on the tooth surface is completely burned. At the same time, measure the tooth thickness reduction to not exceed 10% of the original tooth thickness.

If any of the following conditions occurs, forced repair is not recommended and the meshing gears need to be replaced in pairs: burnt cracks on the tooth surface extend to the tooth root, more than 30% of the tooth surface peeling area, serious tooth shape deformation leading to complete misalignment of the transmission backlash.

3. Post-repair verification and recurrence prevention requirements

Completely drain the old oil, clean all oil circuits, and add TY series standard L-CKD 220# extreme pressure industrial gear oil to the 2/3 position of the oil window.

Gradually load the test run at 50% → 75% → 100% rated load, and monitor the bearing temperature rise throughout the process to not exceed the ambient temperature + 40°C, and the vibration value of the whole machine is ≤ 4.5mm/s.

New oil must be replaced after the first 50 hours of operation, and any metal debris remaining in the repair must be completely removed to avoid secondary scratches on the tooth surface.

FEEDBACK

Pneumatic Conveying Gearbox Market 2027: Blower, Airlock and Screw Drive Demand

摆线针轮减速机两级速比怎么定:组合表怎么读、怎么校核、怎么落到机座号 - 杭州威高传动

Pellet Mill Gearbox Selection: Ring Die Torque, Thermal Rating and VFD Restart

Is there any way to reduce the parallelism error of the reducer?

Let me introduce in detail how to judge whether the worm gear joint surface of PWU160-40-V reducer is damaged.