What are the common problems with NGW42-25 planetary reducer base welding?

Publish Time: 2026-11-12     Origin: Site

1. Common welding defects of the weld body

‌Surface defects‌: pores, undercuts, welding nodules, and spatter residues appear in the weld, mostly caused by the welding material not being dried, the welding current being too high, or not being cleaned properly.

‌Internal defects‌: There are incomplete penetration, slag inclusions, and hidden cracks inside the weld. The root cause is irregular groove processing and incomplete slag removal between multi-layer welding layers.

‌Special Material Defects‌: Cast iron machine bases are prone to produce white, hard and brittle structures during welding, which directly reduces the toughness of the weld and causes subsequent delayed cracking.

2. Welding deformation and shape accuracy are out of tolerance

The key mounting surface of the machine base and the bearing holes were unevenly heated and warped, and the flatness and coaxiality deviation exceeded 0.05mm, resulting in the failure of subsequent planetary gear train assembly accuracy.

Parts where stress is concentrated, such as foot flanges and reinforcing ribs, are partially deformed, gaps appear on the joint surface between the machine base and the equipment base, and the vibration value exceeds the standard during operation.

The long weld was not welded in symmetrical sections, and the overall deformation exceeded the constraint range of the rigid fixed tooling, making it impossible to restore accuracy through subsequent correction.

3. The problem of failure in adapting materials and welding materials

The actual material of the machine base (HT250 cast iron, ZG270-500 cast steel, Q345B low alloy steel) was not distinguished, and ordinary carbon steel electrodes were used incorrectly, resulting in a mismatch in the strength of the weld and the base material.

The low-hydrogen welding rod was not baked at 350°C for 2 hours as required. The welding material absorbed moisture and caused cold cracks in the weld seam, which expanded rapidly after being stressed.

The cast iron machine base did not use special nickel-based welding rods, but was forcibly welded with ordinary carbon steel welding rods. The fusion of the welds was extremely poor, and it cracked again within a short time after repair.

4. Residual stress and hidden dangers of post-weld failure

Without thermal insulation and slow cooling or stress relief annealing after welding, residual stress in the weld and heat-affected zone is concentrated, and secondary cracking occurs under the action of alternating loads during operation.

No crack relief holes were drilled at both ends of the crack before welding. The crack continued to extend during the welding process and the repair scope was out of control.

Precision components such as planet wheels and bearings inside the machine base were not disassembled in advance during welding. High temperature conduction caused permanent damage to the accuracy of the transmission components.

There was no kerosene leakage test after welding, and there were micropores in the weld. The lubricating oil inside the base leaked during operation, causing lubrication failure.

FEEDBACK

Offshore Wind Vessel Gearbox Market 2027: Crane and Winch Drive Demand

How to check the carrying capacity of worm gear reducer: working condition coefficient, efficiency and Selection calculation example - Hangzhou Weigao Transmission

Lubrication and maintenance characteristics of B series industrial gearboxes

What are the common misunderstandings in B series gearbox maintenance?

Apron Feeder Gearbox Selection: Chain Pull, Shock Load and Service Factor